Cargando…

The effect of Er, Cr:YSGG laser debonding on the bond strength of two ceramic materials to dentin

OBJECTIVES: Evaluating the bond strength of two ceramic materials to dentin after Er,Cr:YSGG laser debonding. Would laser debonding affect the bond strength of ceramic to dentin? MATERIALS AND METHODS: Recently extracted human molars were ground to expose dentin. Forty square shaped samples were pre...

Descripción completa

Detalles Bibliográficos
Autores principales: Abdel Sadek, Hoda M., Abdel Khalek, Ahmed M., Wahsh, Marwa M.
Formato: Online Artículo Texto
Lenguaje:English
Publicado: BioMed Central 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9835312/
https://www.ncbi.nlm.nih.gov/pubmed/36635647
http://dx.doi.org/10.1186/s12903-023-02721-9
Descripción
Sumario:OBJECTIVES: Evaluating the bond strength of two ceramic materials to dentin after Er,Cr:YSGG laser debonding. Would laser debonding affect the bond strength of ceramic to dentin? MATERIALS AND METHODS: Recently extracted human molars were ground to expose dentin. Forty square shaped samples were prepared from CAD/CAM ceramic blocks. Samples were divided into two groups according to the type of ceramic material; group E: Lithium disilicate and group T: Ultra-translucent Zirconia (n = 20) Each group was divided into two subgroups (n = 10) according to the laser debonding effect (subgroup B: bonded samples, subgroup R: re-bonded samples after laser debonding). Ceramic samples were bonded to dentin using dual cure self-adhesive resin cement. Laser debonding of ceramic samples of subgroups R using Er, Cr:YSGG laser, were then re-bonded again to dentin surface with same resin cement. The Shear bond strength test using Universal testing machine was done. The failure mode was analyzed. Two-way analysis of variance was used to compare the mean bond strength and re-bond strength of two materials. The significance level was set at P ≤ 0.05. RESULTS: Two-Way ANOVA showed that ceramic type had a significant effect on the re-bond strength to dentin. The predominant failure mode was adhesive. CONCLUSIONS: Laser debonding of Lithium disilicate and Ultra translucent Zirconia decreased the re-bond strength to dentin. Deterioration in re-bond strength for Lithium disilicate ceramics was more pronounced than for Ultra translucent Zirconia. Clinical Relevance Deterioration in the bond strength between ceramics & dentin after laser debonding still needs improvement to allow its clinical use.