Evolution of Structure and Properties of Nickel-Enriched NiTi Shape Memory Alloy Subjected to Bi-Axial Deformation
The effect of a promising method of performing a thermomechanical treatment which provides the nanocrystalline structure formation in bulk NiTi shape memory alloy samples and a corresponding improvement to their properties was studied in the present work. The bi-axial severe plastic deformation of T...
Autores principales: | , , , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9862455/ https://www.ncbi.nlm.nih.gov/pubmed/36676248 http://dx.doi.org/10.3390/ma16020511 |
Sumario: | The effect of a promising method of performing a thermomechanical treatment which provides the nanocrystalline structure formation in bulk NiTi shape memory alloy samples and a corresponding improvement to their properties was studied in the present work. The bi-axial severe plastic deformation of Ti-50.7at.%Ni alloy was carried out on the MaxStrain module of the Gleeble system at 350 and 330 °C with accumulated true strains of e = 6.6–9.5. The obtained structure and its mechanical and functional properties and martensitic transformations were studied using DSC, X-ray diffractometry, and TEM. A nanocrystalline structure with a grain/subgrain size of below 80 nm was formed in bulk nickel-enriched NiTi alloy after the MaxStrain deformation at 330 °C with e = 9.5. The application of MaxStrain leads to the formation of a nanocrystalline structure that is characterized by the appearance of a nano-sized grains and subgrains with equiaxed and elongated shapes and a high free dislocation density. After the MaxStrain deformation at 330 °C with e = 9.5 was performed, the completely nanocrystalline structure with the grain/subgrain size of below 80 nm was formed in bulk nickel-enriched NiTi alloy for the first time. The resulting structure provides a total recoverable strain of 12%, which exceeds the highest values that have been reported for bulk nickel-enriched NiTi samples. |
---|