Cargando…

The Use of Micro-Ribbons and Micro-Fibres in the Formulation of 3D Printed Fast Dissolving Oral Films

Three-dimensional printing (3DP) allows production of novel fast dissolving oral films (FDFs). However, mechanical properties of the films may not be desirable when certain excipients are used. This work investigated whether adding chitosan micro-ribbons or cellulose microfibres will achieve desired...

Descripción completa

Detalles Bibliográficos
Autores principales: Algellay, Marwan, Roberts, Matthew, Bosworth, Lucy, Sarker, Satyajit D., Fatokun, Amos A., Ehtezazi, Touraj
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9862838/
https://www.ncbi.nlm.nih.gov/pubmed/36678576
http://dx.doi.org/10.3390/ph16010079
Descripción
Sumario:Three-dimensional printing (3DP) allows production of novel fast dissolving oral films (FDFs). However, mechanical properties of the films may not be desirable when certain excipients are used. This work investigated whether adding chitosan micro-ribbons or cellulose microfibres will achieve desired FDFs by fused deposition modelling 3DP. Filaments containing polyvinyl alcohol (PVA) and paracetamol as model drug were manufactured at 170 °C. At 130 °C, filaments containing polyvinylpyrrolidone (PVP) and paracetamol were also created. FDFs were printed with plain or mesh patterns at temperatures of 200 °C (PVA) or 180 °C (PVP). Both chitosan micro-ribbons and cellulose micro-fibres improved filament mechanical properties at 1% w/w concentration in terms of flexibility and stiffness. The filaments were not suitable for printing at higher concentrations of chitosan micro-ribbons and cellulose micro-fibres. Furthermore, mesh FDFs containing only 1% chitosan micro-ribbons disintegrated in distilled water within 40.33 ± 4.64 s, while mesh FDFs containing only 7% croscarmellose disintegrated in 55.33 ± 2.86 s, and croscarmellose containing films showed signs of excipient scorching for PVA polymer. Cellulose micro-fibres delayed disintegration of PVA mesh films to 108.66 ± 3.68 s at 1% w/w. In conclusion, only chitosan micro-ribbons created a network of hydrophilic channels within the films, which allowed faster disintegration time at considerably lower concentrations.