Effects of Post-UV-Curing on the Flexural and Absorptive Behaviour of FDM-3D-Printed Poly(lactic acid) Parts

In this study, the effects of the post-ultraviolet-curing process on the flexural, absorptive, and morphological properties of poly(lactic acid) specimens produced using a fused deposition modelling technique 3D printer were experimentally investigated. In this direction, 15, 30, 45, and 60 min post...

Descripción completa

Detalles Bibliográficos
Autor principal: Akderya, Tarkan
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9866767/
https://www.ncbi.nlm.nih.gov/pubmed/36679230
http://dx.doi.org/10.3390/polym15020348
_version_ 1784876173637976064
author Akderya, Tarkan
author_facet Akderya, Tarkan
author_sort Akderya, Tarkan
collection PubMed
description In this study, the effects of the post-ultraviolet-curing process on the flexural, absorptive, and morphological properties of poly(lactic acid) specimens produced using a fused deposition modelling technique 3D printer were experimentally investigated. In this direction, 15, 30, 45, and 60 min post-UV-curing processes were applied to poly(lactic acid) three-point bending and absorption specimens produced at 190 and 200 °C. Three-point bending tests and morphological analyses were applied after the post-ultraviolet-curing process, and absorption tests were applied by immersing the post-ultraviolet-cured specimens in a distilled water bath for 1-, 3-day, and 1-, 2-, and 4-week exposure times. The changes in flexural strain properties for each experimental parameter were also simulated by the computer-aided finite element analysis and compared with the experimental results. It was observed that the post-ultraviolet-curing process increased the flexural strength of the poly(lactic acid) specimens produced at both 190 and 200 °C with the same increasing trend up to 30 min of exposure, and the most significant increase was determined in the specimens that were subjected to post-ultraviolet-curing for 30 min. Although the flexural strengths of the post-ultraviolet-cured specimens were higher than the non-cured specimens in all conditions, it was detected that they tended to decrease after 30 min.
format Online
Article
Text
id pubmed-9866767
institution National Center for Biotechnology Information
language English
publishDate 2023
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-98667672023-01-22 Effects of Post-UV-Curing on the Flexural and Absorptive Behaviour of FDM-3D-Printed Poly(lactic acid) Parts Akderya, Tarkan Polymers (Basel) Article In this study, the effects of the post-ultraviolet-curing process on the flexural, absorptive, and morphological properties of poly(lactic acid) specimens produced using a fused deposition modelling technique 3D printer were experimentally investigated. In this direction, 15, 30, 45, and 60 min post-UV-curing processes were applied to poly(lactic acid) three-point bending and absorption specimens produced at 190 and 200 °C. Three-point bending tests and morphological analyses were applied after the post-ultraviolet-curing process, and absorption tests were applied by immersing the post-ultraviolet-cured specimens in a distilled water bath for 1-, 3-day, and 1-, 2-, and 4-week exposure times. The changes in flexural strain properties for each experimental parameter were also simulated by the computer-aided finite element analysis and compared with the experimental results. It was observed that the post-ultraviolet-curing process increased the flexural strength of the poly(lactic acid) specimens produced at both 190 and 200 °C with the same increasing trend up to 30 min of exposure, and the most significant increase was determined in the specimens that were subjected to post-ultraviolet-curing for 30 min. Although the flexural strengths of the post-ultraviolet-cured specimens were higher than the non-cured specimens in all conditions, it was detected that they tended to decrease after 30 min. MDPI 2023-01-09 /pmc/articles/PMC9866767/ /pubmed/36679230 http://dx.doi.org/10.3390/polym15020348 Text en © 2023 by the author. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Akderya, Tarkan
Effects of Post-UV-Curing on the Flexural and Absorptive Behaviour of FDM-3D-Printed Poly(lactic acid) Parts
title Effects of Post-UV-Curing on the Flexural and Absorptive Behaviour of FDM-3D-Printed Poly(lactic acid) Parts
title_full Effects of Post-UV-Curing on the Flexural and Absorptive Behaviour of FDM-3D-Printed Poly(lactic acid) Parts
title_fullStr Effects of Post-UV-Curing on the Flexural and Absorptive Behaviour of FDM-3D-Printed Poly(lactic acid) Parts
title_full_unstemmed Effects of Post-UV-Curing on the Flexural and Absorptive Behaviour of FDM-3D-Printed Poly(lactic acid) Parts
title_short Effects of Post-UV-Curing on the Flexural and Absorptive Behaviour of FDM-3D-Printed Poly(lactic acid) Parts
title_sort effects of post-uv-curing on the flexural and absorptive behaviour of fdm-3d-printed poly(lactic acid) parts
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9866767/
https://www.ncbi.nlm.nih.gov/pubmed/36679230
http://dx.doi.org/10.3390/polym15020348
work_keys_str_mv AT akderyatarkan effectsofpostuvcuringontheflexuralandabsorptivebehaviouroffdm3dprintedpolylacticacidparts