In Vitro Investigation of Material Combinations for Meso- and Suprastructures in a Biomimetic Approach to Restore One-Piece Zirconia Implants

The aim of this study was to find a suitable material combination to avoid cement excess in the marginal region of one-piece zirconia implant-supported restorations by means of a hybrid crown consisting of a meso- and a suprastructure. One-piece zirconia implants (n = 120) were embedded in epoxy res...

Descripción completa

Detalles Bibliográficos
Autores principales: Nueesch, Reto, Karlin, Sabrina, Fischer, Jens, Rohr, Nadja
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9960926/
https://www.ncbi.nlm.nih.gov/pubmed/36836985
http://dx.doi.org/10.3390/ma16041355
_version_ 1784895629524205568
author Nueesch, Reto
Karlin, Sabrina
Fischer, Jens
Rohr, Nadja
author_facet Nueesch, Reto
Karlin, Sabrina
Fischer, Jens
Rohr, Nadja
author_sort Nueesch, Reto
collection PubMed
description The aim of this study was to find a suitable material combination to avoid cement excess in the marginal region of one-piece zirconia implant-supported restorations by means of a hybrid crown consisting of a meso- and a suprastructure. One-piece zirconia implants (n = 120) were embedded in epoxy resin. Microfilled resin composite mesostructures (n = 60), designed as caps, were bonded on the implant abutment with a primer only. A molar crown was constructed and cemented with a resin cement on top of the mesostructure as a suprastructure out of feldspar ceramic (n = 12), lithium-disilicate (n = 24), or zirconia (n = 24). Fracture load (n = 6) and retention force (n = 6) were measured immediately after storage in distilled water at 37 °C for 24 h, as well as after an additional exposure to artificial aging in a chewing simulator and simultaneous thermal cycling. For the measurement of the fracture load, monolithic crowns made of the employed restorative materials and identical in shape to the hybrid crowns served as controls (n = 6 each). Fracture load values for feldspar ceramic and lithium-disilicate hybrid crowns were slightly higher than those for the respective monolithic crowns at baseline and after aging, which was statistically significant only for feldspar crowns after aging. In contrast, fracture load values for zirconia monolithic crowns were higher than those for zirconia hybrid crowns, which was only statistically significant after aging. Artificial aging reduced the fracture load of feldspar and lithium-disilicate crowns both for hybrid and monolithic crowns. The effect was only statistically significant for lithium disilicate hybrid crowns. The fracture load for hybrid and monolithic zirconia crowns was increased by artificial aging without reaching statistical significance. The retention force of lithium-disilicate and zirconia hybrid crowns was not affected by artificial aging. Taking into account retention force and fracture load, lithium-disilicate hybrid crowns showed promising results.
format Online
Article
Text
id pubmed-9960926
institution National Center for Biotechnology Information
language English
publishDate 2023
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-99609262023-02-26 In Vitro Investigation of Material Combinations for Meso- and Suprastructures in a Biomimetic Approach to Restore One-Piece Zirconia Implants Nueesch, Reto Karlin, Sabrina Fischer, Jens Rohr, Nadja Materials (Basel) Article The aim of this study was to find a suitable material combination to avoid cement excess in the marginal region of one-piece zirconia implant-supported restorations by means of a hybrid crown consisting of a meso- and a suprastructure. One-piece zirconia implants (n = 120) were embedded in epoxy resin. Microfilled resin composite mesostructures (n = 60), designed as caps, were bonded on the implant abutment with a primer only. A molar crown was constructed and cemented with a resin cement on top of the mesostructure as a suprastructure out of feldspar ceramic (n = 12), lithium-disilicate (n = 24), or zirconia (n = 24). Fracture load (n = 6) and retention force (n = 6) were measured immediately after storage in distilled water at 37 °C for 24 h, as well as after an additional exposure to artificial aging in a chewing simulator and simultaneous thermal cycling. For the measurement of the fracture load, monolithic crowns made of the employed restorative materials and identical in shape to the hybrid crowns served as controls (n = 6 each). Fracture load values for feldspar ceramic and lithium-disilicate hybrid crowns were slightly higher than those for the respective monolithic crowns at baseline and after aging, which was statistically significant only for feldspar crowns after aging. In contrast, fracture load values for zirconia monolithic crowns were higher than those for zirconia hybrid crowns, which was only statistically significant after aging. Artificial aging reduced the fracture load of feldspar and lithium-disilicate crowns both for hybrid and monolithic crowns. The effect was only statistically significant for lithium disilicate hybrid crowns. The fracture load for hybrid and monolithic zirconia crowns was increased by artificial aging without reaching statistical significance. The retention force of lithium-disilicate and zirconia hybrid crowns was not affected by artificial aging. Taking into account retention force and fracture load, lithium-disilicate hybrid crowns showed promising results. MDPI 2023-02-05 /pmc/articles/PMC9960926/ /pubmed/36836985 http://dx.doi.org/10.3390/ma16041355 Text en © 2023 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Nueesch, Reto
Karlin, Sabrina
Fischer, Jens
Rohr, Nadja
In Vitro Investigation of Material Combinations for Meso- and Suprastructures in a Biomimetic Approach to Restore One-Piece Zirconia Implants
title In Vitro Investigation of Material Combinations for Meso- and Suprastructures in a Biomimetic Approach to Restore One-Piece Zirconia Implants
title_full In Vitro Investigation of Material Combinations for Meso- and Suprastructures in a Biomimetic Approach to Restore One-Piece Zirconia Implants
title_fullStr In Vitro Investigation of Material Combinations for Meso- and Suprastructures in a Biomimetic Approach to Restore One-Piece Zirconia Implants
title_full_unstemmed In Vitro Investigation of Material Combinations for Meso- and Suprastructures in a Biomimetic Approach to Restore One-Piece Zirconia Implants
title_short In Vitro Investigation of Material Combinations for Meso- and Suprastructures in a Biomimetic Approach to Restore One-Piece Zirconia Implants
title_sort in vitro investigation of material combinations for meso- and suprastructures in a biomimetic approach to restore one-piece zirconia implants
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9960926/
https://www.ncbi.nlm.nih.gov/pubmed/36836985
http://dx.doi.org/10.3390/ma16041355
work_keys_str_mv AT nueeschreto invitroinvestigationofmaterialcombinationsformesoandsuprastructuresinabiomimeticapproachtorestoreonepiecezirconiaimplants
AT karlinsabrina invitroinvestigationofmaterialcombinationsformesoandsuprastructuresinabiomimeticapproachtorestoreonepiecezirconiaimplants
AT fischerjens invitroinvestigationofmaterialcombinationsformesoandsuprastructuresinabiomimeticapproachtorestoreonepiecezirconiaimplants
AT rohrnadja invitroinvestigationofmaterialcombinationsformesoandsuprastructuresinabiomimeticapproachtorestoreonepiecezirconiaimplants