Cargando…
Forming Limit Analysis of Thin-Walled Extruded Aluminum Alloy Tubes under Nonlinear Loading Paths Using an Improved M-K Model
To meet the requirement of lighter weight and better performance in tube hydroforming, one of the most important tasks is to accurately predict the forming limit of thin-walled tubes under nonlinear loading paths. This work established the M-K+DF2012 model, a combination of the M-K model and the DF2...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9966077/ https://www.ncbi.nlm.nih.gov/pubmed/36837273 http://dx.doi.org/10.3390/ma16041647 |
_version_ | 1784896926339039232 |
---|---|
author | Zhu, Haihui Lin, Yanli Chen, Kelin He, Zhubin |
author_facet | Zhu, Haihui Lin, Yanli Chen, Kelin He, Zhubin |
author_sort | Zhu, Haihui |
collection | PubMed |
description | To meet the requirement of lighter weight and better performance in tube hydroforming, one of the most important tasks is to accurately predict the forming limit of thin-walled tubes under nonlinear loading paths. This work established the M-K+DF2012 model, a combination of the M-K model and the DF2012 ductile fracture criterion, for the forming limit prediction of thin-walled tubes under nonlinear loading paths. In this model, the failure of the groove is determined by the DF2012 criterion, and the corresponding strains in the uniform region are the limit strains. The limit strains of an AA6061 aluminum alloy tube under a set of linear loading paths and two typical nonlinear loading paths were tested. Parameter values of the M-K+DF2012 model for the tube were determined based on the experimental limit strains under linear loading paths, and the limit strains under the two nonlinear loading paths were predicted. Then the strain-based forming limit diagram (ε-FLD) and the polar effective plastic strain FLD (PEPS-FLD) of the tube under different pre-strains were predicted and discussed. The results show that the limit strains of the tube are obviously path-dependent, and the M-K+DF2012 model can reasonably capture the limit strains of the tube under both linear and nonlinear loading paths. The predicted ε-FLD shows a strong dependence on the pre-strain, while the predicted PEPS-FLD is weakly strain path-dependent and almost path-independent on the right-hand side for the AA6061 tube. |
format | Online Article Text |
id | pubmed-9966077 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2023 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-99660772023-02-26 Forming Limit Analysis of Thin-Walled Extruded Aluminum Alloy Tubes under Nonlinear Loading Paths Using an Improved M-K Model Zhu, Haihui Lin, Yanli Chen, Kelin He, Zhubin Materials (Basel) Article To meet the requirement of lighter weight and better performance in tube hydroforming, one of the most important tasks is to accurately predict the forming limit of thin-walled tubes under nonlinear loading paths. This work established the M-K+DF2012 model, a combination of the M-K model and the DF2012 ductile fracture criterion, for the forming limit prediction of thin-walled tubes under nonlinear loading paths. In this model, the failure of the groove is determined by the DF2012 criterion, and the corresponding strains in the uniform region are the limit strains. The limit strains of an AA6061 aluminum alloy tube under a set of linear loading paths and two typical nonlinear loading paths were tested. Parameter values of the M-K+DF2012 model for the tube were determined based on the experimental limit strains under linear loading paths, and the limit strains under the two nonlinear loading paths were predicted. Then the strain-based forming limit diagram (ε-FLD) and the polar effective plastic strain FLD (PEPS-FLD) of the tube under different pre-strains were predicted and discussed. The results show that the limit strains of the tube are obviously path-dependent, and the M-K+DF2012 model can reasonably capture the limit strains of the tube under both linear and nonlinear loading paths. The predicted ε-FLD shows a strong dependence on the pre-strain, while the predicted PEPS-FLD is weakly strain path-dependent and almost path-independent on the right-hand side for the AA6061 tube. MDPI 2023-02-16 /pmc/articles/PMC9966077/ /pubmed/36837273 http://dx.doi.org/10.3390/ma16041647 Text en © 2023 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Zhu, Haihui Lin, Yanli Chen, Kelin He, Zhubin Forming Limit Analysis of Thin-Walled Extruded Aluminum Alloy Tubes under Nonlinear Loading Paths Using an Improved M-K Model |
title | Forming Limit Analysis of Thin-Walled Extruded Aluminum Alloy Tubes under Nonlinear Loading Paths Using an Improved M-K Model |
title_full | Forming Limit Analysis of Thin-Walled Extruded Aluminum Alloy Tubes under Nonlinear Loading Paths Using an Improved M-K Model |
title_fullStr | Forming Limit Analysis of Thin-Walled Extruded Aluminum Alloy Tubes under Nonlinear Loading Paths Using an Improved M-K Model |
title_full_unstemmed | Forming Limit Analysis of Thin-Walled Extruded Aluminum Alloy Tubes under Nonlinear Loading Paths Using an Improved M-K Model |
title_short | Forming Limit Analysis of Thin-Walled Extruded Aluminum Alloy Tubes under Nonlinear Loading Paths Using an Improved M-K Model |
title_sort | forming limit analysis of thin-walled extruded aluminum alloy tubes under nonlinear loading paths using an improved m-k model |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9966077/ https://www.ncbi.nlm.nih.gov/pubmed/36837273 http://dx.doi.org/10.3390/ma16041647 |
work_keys_str_mv | AT zhuhaihui forminglimitanalysisofthinwalledextrudedaluminumalloytubesundernonlinearloadingpathsusinganimprovedmkmodel AT linyanli forminglimitanalysisofthinwalledextrudedaluminumalloytubesundernonlinearloadingpathsusinganimprovedmkmodel AT chenkelin forminglimitanalysisofthinwalledextrudedaluminumalloytubesundernonlinearloadingpathsusinganimprovedmkmodel AT hezhubin forminglimitanalysisofthinwalledextrudedaluminumalloytubesundernonlinearloadingpathsusinganimprovedmkmodel |