Cargando…
Texture and Magnetic Property of Fe-6.5 wt % Si Steel Strip with Cu-Rich Particles Modification
[Image: see text] Based on the ordered phase effectively suppressed by rapid solidification technology, the grain refinement concept using Cu is incorporated into the soft magnetic materials. Cu dosage not only could refine the grain size with an average grain size of 8.7 μm but also improve the con...
Autores principales: | Zhang, Di, Su, Yingtao, Yang, Xingrui, Sun, Huilan, Guo, Zhihong, Wang, Bo, Ma, Cheng, Dong, Zhongqi, Zhu, Liguang |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
American Chemical Society
2023
|
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9996763/ https://www.ncbi.nlm.nih.gov/pubmed/36910929 http://dx.doi.org/10.1021/acsomega.2c07510 |
Ejemplares similares
-
Characterization of the Fe-6.5wt%Si Strip with Rapid
Cooling Coupling Deep Supercooled Solidification
por: Wang, Bo, et al.
Publicado: (2021) -
Influence of Process Parameters on Grain Size and Texture Evolution of Fe-3.2 wt.-% Si Non-Oriented Electrical Steels
por: Wei, Xuefei, et al.
Publicado: (2021) -
Effect of Cold Rolling Process on Microstructure, Texture and Properties of Strip Cast Fe-2.6%Si Steel
por: Xu, Yunbo, et al.
Publicado: (2018) -
Characterization and Calculation of the Dynamic Recrystallization Texture in Fe-3.0 Wt.% Si Alloy
por: Shao, Guangshuai, et al.
Publicado: (2022) -
On the through-process texture evolution assessment in grain oriented Fe-3 wt% Si steel produced by a novel directional inoculation technique
por: Tripathy, Snehashish, et al.
Publicado: (2021)