801“…Results showed that hydroxyapatite catalyst pore size reduced with increasing the calcination temperature. Optimize biodiesel yield (89 wt%) was achieved through the process of transesterification with optimum reaction conditions of 4 wt% catalyst, oil to ethanol molar ratio of 1:7 and temperature 75 °C for 3 h reaction time. …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
802por Okonkwo, Chinwe P., Ajiwe, Vincent I. E., Ikeuba, Alexander I., Emori, Wilfred, Okwu, Modestus O., Ayogu, Jude I.“…This study presents an approach to produce biodiesel from Elaeis guineensis using natural heterogeneous catalysts derived from raw, calcined, and acid-activated forms of waste snail shells. …”
Publicado 2023
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
803“…This investigation tried seeking a new approach to reuse them to high quality, including turning PG into calcinated PG (CPG) via washing and calcination, as well as adopting sodium metasilicate nonahydrate (SMN) to strengthen the roadbase materials of cement-stabilized CPG and RCA. …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
804“…The effects of the calcination temperature, ratio, initial methylene blue (MB) concentration, and catalyst dosage on the adsorption and photocatalytic performance were investigated. …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
805por Wang, Qingqing, Peng, Lin, Li, Guohui, Zhang, Ping, Li, Dawei, Huang, Fenglin, Wei, Qufu“…The pristine MMT and TiO(2)-MMT calcined at 800 °C (TiO(2)-MMT800) were used for comparison to better understand the immobilization mechanism. …”
Publicado 2013
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
806“…Here, we provide new, direct radiocarbon and physico-chemical analyses on calcined bones which elucidates the complex depositional history of the assemblage. …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
807“…The sediment in a malodorous river (PS) in Beijing, China was selected and modified via calcination (PS-D), Na(+) doping (PS-Na) and calcination–Na(+) doping (PS-DNa). …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
808por Accardo, Grazia, Dell’Agli, Gianfranco, Mascolo, Maria Cristina, Spiridigliozzi, Luca, Yoon, Sung Pil“…The amorphous powders, upon a mild calcination step, gave rise to the formation of stable solid solutions of fluorite-structured ceria maintaining the same morphology of the starting powders. …”
Publicado 2019
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
809por Lin, Hanzhi, Chen, Tao, Yan, Bo, Huang, Zulv, Zhou, Yang, Huang, Jian, Xiao, Xianming“…The results showed that the activating agent destroyed the crystal structure of the quartz sand under calcination, and formed Si-O-Na and Si-OH groups to realize activation. …”
Publicado 2020
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
810por Zhu, Hongguang, Yang, Sen, Li, Weijian, Li, Zonghui, Fan, Jingchong, Shen, Zhengyan“…The ratio of coal gangue (calcined and uncalcined) coarse aggregate replacing the gravel was 0%, 30%, 50%, 70%, and 100%. …”
Publicado 2020
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
811“…Cobalt oxide nanoparticles (CoO NPs) were synthesized by the calcination method from the Co (II) complex which has the formula [Co(PVA)(P-ABA)(H(2)O)(3)], PVA = polyvinyl alcohol, and P-ABA = para-aminobenzoic acid. …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
812“…Besides silica fume, three different types of calcined clays were investigated as SCMs. These were a relatively pure metakaolin, a quartz-rich metakaolin, and a mixed calcined clay, where the amount of other types of clays was two times higher than the kaolinite content. …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
813“…The results show that the novel SAC-MKPC that was prepared from aluminum slag, carbide slag, coal gangue, and magnesium desulfurization slag was composed mainly of mineral MgO, [Formula: see text] , and C(2)S and the calcination temperature of the main mineral phases was 1250–1350 °C. …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
814por Zhang, Ying, Xu, Ruidong, Qin, Ziyang, Feng, Suyang, Wang, Wenbin, Chen, Chen, Ju, Ao“…NiO, Ni–Co–Mn–O(x) and NiO/Ni–Co–Mn–O(x) on nickel foam substrates were prepared via a chemical bath deposition–calcination. The thermodynamic behavior was observed by TG/DTA. …”
Publicado 2020
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
815por Chen, Xiaopeng, Ren, Lu, Yaseen, Muhammad, Wang, Linlin, Liang, Jiezhen, Liang, Ruixue, Chen, Xiankun, Guo, Huiqing“…Optimum conditions for catalyst preparation were obtained as: 15% Ni loading, 723 K calcination temperature, and 723 K reduction temperature for 2.5 h. …”
Publicado 2019
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
816“…Graphitic carbon nitride (g-C(3)N(4)) was prepared by high-temperature calcination of urea. A mixture of g-C(3)N(4) and nano-ZrO(2) precursor was directly calcined to prepare g-C(3)N(4)/ZrO(2) hybrid photocatalysts. …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
817“…These alkoxides were calcined at 400 °C to prepare the oxide catalysts (named as TiEt400 and TiPr400). …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
818“…The eluting efficiency of HCl was 97.5%, and the optimal parameters of the precipitation and calcination processes were set as pH 5, NH(4)Cl:V = 2:1, and 350 °C. …”
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
819por Lagunas-Chavarría, Anggel, Navarro-Rojero, María Guadalupe, Salvador, María Dolores, Benavente, Rut, Catalá-Civera, Jose Manuel, Borrell, Amparo“…X-ray diffraction of the powders calcined by the microwave process shows the formation of perovskite structure with orthorhombic geometry, but it is possible to observe the presence of other phases. …”
Publicado 2022
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto -
820por Kljajević, Ljiljana, Nenadović, Miloš, Ivanović, Marija, Bučevac, Dušan, Mirković, Miljana, Mladenović Nikolić, Nataša, Nenadović, Snežana“…Metakaolin was obtained by calcination of kaolin at 750 °C for 1 h while geopolymer samples were calcined at 900 °C, which is the key transition temperature. …”
Publicado 2022
Enlace del recurso
Enlace del recurso
Enlace del recurso
Online Artículo Texto