  1. 1661
    “…Herein, short-range amorphous nitrogen-doped carbon nanosheets (NCS) coupled with partially graphitized porous carbon architecture were reported, and were prepared via flexible salt-assisted calcination strategy and followed by a simple cleaning process. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  2. 1662
    “…Scaffolds were successfully coated by dipping the sintered samples in a hydroxyapatite (HA) alcoholic suspension, after optimizing the HA solid loading at 20 wt%. After calcination at 1300 °C, the coating layer, composed of a mixture of HA and β-TCP (β-TriCalcium Phospate) adhered well to the zirconia substrate. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  3. 1663
    “…Polyvinyl alcohol/beryllium sulfate/polyethyleneimine (PVA/BeSO(4)/PEI) precursor nanofibers (NFs) was first fabricated to obtain PVA/BeSO(4)/PEI electrospun NFs by electrospinning technology, finally manufactured beryllium oxide (BeO) NFs followed by various heat treatment methods. The minimum calcination temperature for pure BeO NFs was 1000 °C, and the minimum specific surface area (5.1 m(2) g(−1)) and pore volumes (0.0128 cm(3) g(−1)) were at 1300 °C. 46.18% Be and 53.82% O was measured in BeO NFs by X-ray photoelectron spectroscopy. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  4. 1664
    “…In the present study, a promising flowsheet is proposed for REEs recovery from NdFeB magnets, as follows: (1) acid baking, (2) employment of ultrasound-assisted water leaching, (3) the production of rare earth oxides (RE oxides) by a solution combustion method, and (4) a calcination process. There are several problems in conventional precipitation such as loss of a high amount of metal during precipitation and use of a high amount of precipitation agents. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  5. 1665
    “…To determine the optimal synthesis method, X-ray diffraction patterns were obtained and showed that single phase LaFeO(3) with good crystallinity was prepared by the molten salt method after calcination at 600 °C for 4 h. SEM and TEM images showed that the M-LF-600 catalyst preserved the spherical structure of α-Fe(2)O(3) template. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  6. 1666
    “…Further experiments were performed with a 5.0% dilute sulfuric acid solution used to leach a Ti-bearing blast furnace slag sample that had been calcined with concentrated sulfuric acid, at a liquid–solid ratio of 10, a reaction time of 60 min, and a reaction temperature of 338.15 K (65 °C). …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  7. 1667
    “…Through a facile hydrothermal technique, five metal sources are uniformly integrated into amorphous carbon spheres, which are transformed to crystalline HEMOs after calcination. Importantly, by controlling ion diffusion and oxidation rates, HEMOs with different structures can be controllably achieved. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  8. 1668
    “…In this article, we report the fabrication of a Z-scheme P–TiO(2)/g-C(3)N(4) (CNPT-X) heterostructure by the calcination method. Under simulated sunlight, CNPT-X composites are found to show excellent degradation performance against sulfonamide antibiotics sulfadiazine (SD), sulfamethazine (SM2), sulfamonomethoxine (SMM), and sulfamethoxazole (SMZ). …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  9. 1669
    “…In most cases, V and Ni are recovered as thermally decomposable compounds that undergo calcination to produce V(2)O(5) and NiO. Eventually, V and Ni are recovered as pure oxides in most approaches, but pure metals are obtained in exceptional procedures.…”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  10. 1670
    “…In this study, cerium dioxide was prepared through calcination of ceric nitrate and fully characterized using X-ray powder diffraction (XRPD), infrared spectrometry (FT-IR), scanning and transmission electron microscopy (SEM and TEM), thermogravimetric and differential thermal analysis (TG and DTA), dynamic light scattering (DLS), and analysis of surface area. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  11. 1671
    “…The most optimal crystal structure and morphology of TmVO4 have been determined and optimized by varying Schiff-base ligands, the molar ratio of H2Salen, the sonication time and power, and the calcination time. A Eriochrome Black T (EBT) analysis revealed that the specific surface area was 24.91 m2/g. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  12. 1672
    “…The aim of this work is to investigate the possibility of reusing ashes obtained by the calcination of industrial sludge from the oil refining industry (ORSA) as a secondary raw material in the manufacture of alkaline activated cements or geopolymers. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  13. 1673
    “…Ferritin dissolved in deionized water was uniformly dispersed on the Al(2)O(3) surface and calcinated to obtain iron nanoparticles. The synthesis temperature, time, and rotation speed of the chamber were the main parameters used to investigate the growth behavior of CNTs. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  14. 1674
    “…Herein, this work reports metal–organic frameworks (MOFs)-derived cobalt oxide/carbon nanotubes (MWCNTx@Co(3)O(4)) composites by calcining the MWCNTx@ZIF-67 precursor in one step. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  15. 1675
    “…However, the partial oxidation of MXene after calcination could reduce its conductivity. To address this issue, herein, PEDOT:PSS films were introduced to disperse the TiO(2)-MXene materials. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  16. 1676
    “…This research work reports the usability of binary additive materials known as tile waste dust (TWD) and calcined kaolin (CK) in ameliorating the mechanical response of weak soil. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  17. 1677
    “…To avoid leaching, Φy was calcinated, forming a mixed metal oxide (MMO). In the combination of MMO/PMS, no metals leached, the CIP adsorption was low (<20%), and the action of SO(4)•(−) dominated, leading to a synergistic effect on pollutant elimination (>95% after 15 min of treatment). …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  18. 1678
    “…SiC can be grown in situ on the surface of a carbonized wood cell wall by mixing and calcination of wood and Si powder. The samples were characterized using XRD, SEM, and SEM–EDS analysis. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  19. 1679
    “…Hierarchical faujasite was then achieved through calcination and template removal. Subsequently, it was functionalized with ionic liquid and used for the immobilization of heteropolyacid. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto
  20. 1680
    “…The preparation of tablets containing Mg (8.44 mol%) and Zn (2.63 mol%) β-tricalcium phosphate involved biomimetic precipitation of amorphous calcium phosphate in media of simulated body fluid enriched with Mg(2+) and Zn(2+) ions as well as the presence of valine as an organic additive, followed by step-wise calcination up to 1000 °C. The results from laser processing showed formation of deeper patterns with increased surface roughness (from 4.9 µm to 9.4 µm) as laser power and velocity increase, keeping constant the hatch sizes of 50 µm. …”
    Enlace del recurso
    Enlace del recurso
    Enlace del recurso
    Online Artículo Texto