Mechanical Properties and Strain-Induced Filament Degradation of Ex Situ and In Situ $MgB_{2}Wires$
We have compared the mechanical properties and the degradation of the critical current after uniaxial tensile loading at room temperature (RT) and at 77 K of ex situ and in situ $MgB_2$ wires. The strain that the wires can withstand without degradation is at 77 K substantially higher than at RT. In...