Preliminary Results from Validation Measurements of the Longitudinal Power Deposition Model for the LHC Injection Kicker Magnet
During Run 1 of the LHC, one of the injection kicker magnets (MKIs) exhibited an excessively high ferrite temperature, caused by coupling of the high intensity beam to the real impedance of the magnet. Beam-screen upgrades, implemented during Long Shutdown 1 (LS1), have been very effective in reduci...