Cargando…

Influence of TiO(2), Al(2)O(3), and Basicity on Viscosity and Structure of High Titanium-Bearing Blast Furnace Slag

The viscosity of high-titanium blast furnace slag with different TiO(2) content, Al(2)O(3) content, and basicity was measured at 1653–1773 K using the rotational cylinder method. The phase composition of the slag is measured by XRD. Phase diagram of the slags is calculated by FactSage software. Ioni...

Descripción completa

Detalles Bibliográficos
Autores principales: Zhou, Wenbo, Li, Tingle, Lan, Dong, Sun, Changyu, Yang, Songtao
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10095886/
https://www.ncbi.nlm.nih.gov/pubmed/37048874
http://dx.doi.org/10.3390/ma16072575