Effect of Iron Component on the Structural Evolution of Carbon Bonds in Hydrochloric Acid-Demineralized Lignite During Pyrolysis

[Image: see text] The pyrolysis characteristics of hydrochloric acid-demineralized Shengli lignite (SL(+)) and iron-added lignite (SL(+)-Fe) were investigated using a fixed-bed reactor. The primary gaseous products (CO(2), CO, H(2), and CH(4)) were detected via gas chromatography. Fourier-transform...