A Semi-Empirical Damage Model of Helankou Rocks Based on Acoustic Emission

The Helankou rock as the relics carrier in Ningxia, China, have been suffering from serious weathering caused by variable environmental conditions. To study the freeze-thaw damage characteristics of Helankou relics carrier rocks, three dry-wet conditions (i.e., drying, pH = 2 and pH = 7) together wi...