Impact Behaviour of Steel-Fibre-Reinforced Alkali-Activated Slag Concrete Exposed to Elevated Temperatures

Concrete protective structures are mainly meant to withstand impact loads. However, fire events weaken concrete and reduce its impact resistance. This study investigated the impact behaviour of steel-fibre-reinforced alkali-activated slag (AAS) concrete before and after exposure to elevated temperat...