Effect of Prior Boriding on Microstructure and Mechanical Properties of Nanobainitic X37CrMoV5-1 Hot-Work Tool Steel

The influence of prior pack boriding on the microstructure and properties of nanobainitised X37CrMoV5-1 hot-work tool steel was investigated in the present work. Pack boriding was conducted at 950 °C for 4 h. Nanobainitising consisted of two-step isothermal quenching at 320 °C for 1 h, followed by a...