Impact of thermal oxidation parameters on micro-hardness and hot corrosion of Ti-6Al-3Mo-2Nb-2Sn-2Zr-1.5Cr alloy
Protective oxide layers on Ti-6Al-3Mo-2Nb-2Sn-2Zr-1.5Cr (TC21) alloy with equiaxed microstructure considerably influence micro-hardness and hot corrosion resistance. The present work’s thermal oxidation of TC21 alloy was performed at 600, 700, and 800 °C for 5, 20, and 50 h durations. Hot corrosion...