Material Characterization of Polypropylene and Polystyrene Regarding Molecular Degradation Behavior

During the processing of thermoplastics, polymers are subjected to high stress. As a result of this stress, the polymer chains break, leading to a lower molar mass. This further leads to a lower viscosity of the plastic melt and, eventually, to poorer mechanical properties of the manufactured plasti...