Ceramic‐on‐Ceramic or Metal‐on‐Polyethylene: The Bearing of Choice after Ceramic Component Fracture in Total Hip Arthroplasty along with Concise Follow‐Up of the Previous Cohort
OBJECTIVE: We previously reported the questionable result of reoperation using metal‐on‐polyethylene (MoP) bearing after the fracture of the ceramic component. After the report, we abandoned the use of MoP; instead, we used ceramic‐on‐ceramic (CoC) bearing. This report aimed to present the outcome o...