Effect of preheating of low shrinking resin composite on intrapulpal temperature and microtensile bond strength to dentin
The effect of preheating of the silorane-based resin composite on intrapulpal temperature (IPT) and dentin microtensile bond strength (μTBS) was evaluated. For the IPT, teeth (n = 15) were sectioned to obtain discs of 0.5 mm thickness (2 discs/tooth). The discs were divided into three groups (n = 10...