Microstructure and Mechanical Properties of Microwave Sintered ZrO(2) Bioceramics with TiO(2) Addition

The microwave sintered zirconia ceramics with 0, 1, 3, and 5 wt% TiO(2) addition at a low sintering temperature of 1300°C and a short holding time of 1 hour were investigated. Effect of contents of TiO(2) addition on microstructure and mechanical properties of microwave sintered zirconia bioceramics...