Cargando…
Microstructure and Mechanical Properties of Microwave Sintered ZrO(2) Bioceramics with TiO(2) Addition
The microwave sintered zirconia ceramics with 0, 1, 3, and 5 wt% TiO(2) addition at a low sintering temperature of 1300°C and a short holding time of 1 hour were investigated. Effect of contents of TiO(2) addition on microstructure and mechanical properties of microwave sintered zirconia bioceramics...
Autores principales: | Kuo, Hsien-Nan, Chou, Jyh-Horng, Liu, Tung-Kuan |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Hindawi Publishing Corporation
2016
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC4967666/ https://www.ncbi.nlm.nih.gov/pubmed/27504072 http://dx.doi.org/10.1155/2016/2458685 |
Ejemplares similares
-
Improved Microstructure and Hardness Properties of Low-Temperature Microwave-Sintered Y(2)O(3) Stabilized ZrO(2) Ceramics with Additions of Nano TiO(2) Powders
por: Weng, Min-Hang, et al.
Publicado: (2020) -
Study of the Embryonic Toxicity of TiO(2) and ZrO(2) Nanoparticles
por: Lyashenko, Elena Nikolaevna, et al.
Publicado: (2023) -
Significant improvement in TiO(2) photocatalytic activity through controllable ZrO(2) deposition
por: Wang, Xiaofeng, et al.
Publicado: (2018) -
Synthesis of Mixed-Phase TiO(2)–ZrO(2) Nanocomposite for Photocatalytic Wastewater Treatment
por: Kumari, Pooja, et al.
Publicado: (2023) -
The Effect of ZrO(2) Nanoparticles on the Microstructure and Properties of Sintered WC–Bronze-Based Diamond Composites
por: Sun, Youhong, et al.
Publicado: (2016)