ZT > 0.1 Electron‐Carrying Polymer Thermoelectric Composites with In Situ SnCl(2) Microstructure Growth
An n‐type pyromellitic diimide polymer composite with in situ microstructure growth of the common element compound SnCl(2) reaches power factor of 50–100 μW m(−1) K(−2), the highest purely n‐type polymer composite power factor yet reported. The composite has a gigantic Seebeck coefficient between −4...