Threshold intensity factors as lower boundaries for crack propagation in ceramics
BACKGROUND: Slow crack growth can be described in a v (crack velocity) versus K(I )(stress intensity factor) diagram. Slow crack growth in ceramics is attributed to corrosion assisted stress at the crack tip or at any pre-existing defect in the ceramic. The combined effect of high stresses at the cr...