Improvement in the Tensile Bond Strength between 3Y-TZP Ceramic and Enamel by Surface Treatments

This study examined the effects of 3 mol % yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP) ceramic surface treatments on the tensile bond strength and surface characteristics of enamel. To measure the tensile bond strength, the 3Y-TZP and tooth specimens were manufactured in a mini-dumbbe...