High corrosion resistance and weak corrosion anisotropy of an as-rolled Mg-3Al-1Zn (in wt.%) alloy with strong crystallographic texture

Combining with electrochemical corrosion measurements, immersion and hydrogen evolution testing performed in 0.9 wt.% NaCl solution at 37 °C, the corrosion resistance of an as-rolled Mg-3%Al-1%Zn alloy before and after a 3% compressive strain along the rolling direction was investigated. Results rev...