Tailoring Lattice Strain and Ferroelectric Polarization of Epitaxial BaTiO(3) Thin Films on Si(001)

Ferroelectric BaTiO(3) films with large polarization have been integrated with Si(001) by pulsed laser deposition. High quality c-oriented epitaxial films are obtained in a substrate temperature range of about 300 °C wide. The deposition temperature critically affects the growth kinetics and thermod...