Delayed degradation according to the location of fixation with using an absorbable plate
BACKGROUND: The ideal absorbable plating system should provide sufficient rigidity and then be absorbed within a timely manner. The Resorb-X has been recently developed as a plating system with a mixture ratio of 50:50 poly(D, L-lactide). METHODS: We present seven of 121 patients who experienced del...