Investigation of the Influence of Pre-Charged Hydrogen on Fracture Toughness of As-Received 2.25Cr1Mo0.25V Steel and Weld

Fracture failure caused by hydrogen embrittlement (HE) is a major concern for the system reliability and safety of hydrogen storage vessels, which are generally made of 2.25Cr1Mo0.25V steel. Thus, study of the influence of pre-charged hydrogen on fracture toughness of as-received 2.25Cr1Mo0.25V stee...