Low Temperature Hot Corrosion Screening of Single Crystal Superalloys

Single crystal superalloys were screened in Type II molten (Na,K)-sulfate hot corrosion re-coat tests in air +300 ppm SO(2) at 700 °C. They exhibited large 20–40 mg/cm(2) weight changes, repeated spallation, and non-protective, 25–50 μm thick corrosion layers after 300 h of testing. Scale cross sect...

Descripción completa