Bonding Strength of a Glass Microfluidic Device Fabricated by Femtosecond Laser Micromachining and Direct Welding

We present a rapid and highly reliable glass (fused silica) microfluidic device fabrication process using various laser processes, including maskless microchannel formation and packaging. Femtosecond laser assisted selective etching was adopted to pattern microfluidic channels on a glass substrate a...

Descripción completa

Detalles Bibliográficos
Autores principales: Kim, Sungil, Kim, Jeongtae, Joung, Yeun-Ho, Choi, Jiyeon, Koo, Chiwan
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2018
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6315772/
https://www.ncbi.nlm.nih.gov/pubmed/30513880
http://dx.doi.org/10.3390/mi9120639
_version_ 1783384374080700416
author Kim, Sungil
Kim, Jeongtae
Joung, Yeun-Ho
Choi, Jiyeon
Koo, Chiwan
author_facet Kim, Sungil
Kim, Jeongtae
Joung, Yeun-Ho
Choi, Jiyeon
Koo, Chiwan
author_sort Kim, Sungil
collection PubMed
description We present a rapid and highly reliable glass (fused silica) microfluidic device fabrication process using various laser processes, including maskless microchannel formation and packaging. Femtosecond laser assisted selective etching was adopted to pattern microfluidic channels on a glass substrate and direct welding was applied for local melting of the glass interface in the vicinity of the microchannels. To pattern channels, a pulse energy of 10 μJ was used with a scanning speed of 100 mm/s at a pulse repetition rate of 500 kHz. After 20–30 min of etching in hydrofluoric acid (HF), the glass was welded with a pulse energy of 2.7 μJ and a speed of 20 mm/s. The developed process was as simple as drawing, but powerful enough to reduce the entire production time to an hour. To investigate the welding strength of the fabricated glass device, we increased the hydraulic pressure inside the microchannel of the glass device integrated into a custom-built pressure measurement system and monitored the internal pressure. The glass device showed extremely reliable bonding by enduring internal pressure up to at least 1.4 MPa without any leakage or breakage. The measured pressure is 3.5-fold higher than the maximum internal pressure of the conventional polydimethylsiloxane (PDMS)–glass or PDMS–PDMS bonding. The demonstrated laser process can be applied to produce a new class of glass devices with reliability in a high pressure environment, which cannot be achieved by PDMS devices or ultraviolet (UV) glued glass devices.
format Online
Article
Text
id pubmed-6315772
institution National Center for Biotechnology Information
language English
publishDate 2018
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-63157722019-01-10 Bonding Strength of a Glass Microfluidic Device Fabricated by Femtosecond Laser Micromachining and Direct Welding Kim, Sungil Kim, Jeongtae Joung, Yeun-Ho Choi, Jiyeon Koo, Chiwan Micromachines (Basel) Article We present a rapid and highly reliable glass (fused silica) microfluidic device fabrication process using various laser processes, including maskless microchannel formation and packaging. Femtosecond laser assisted selective etching was adopted to pattern microfluidic channels on a glass substrate and direct welding was applied for local melting of the glass interface in the vicinity of the microchannels. To pattern channels, a pulse energy of 10 μJ was used with a scanning speed of 100 mm/s at a pulse repetition rate of 500 kHz. After 20–30 min of etching in hydrofluoric acid (HF), the glass was welded with a pulse energy of 2.7 μJ and a speed of 20 mm/s. The developed process was as simple as drawing, but powerful enough to reduce the entire production time to an hour. To investigate the welding strength of the fabricated glass device, we increased the hydraulic pressure inside the microchannel of the glass device integrated into a custom-built pressure measurement system and monitored the internal pressure. The glass device showed extremely reliable bonding by enduring internal pressure up to at least 1.4 MPa without any leakage or breakage. The measured pressure is 3.5-fold higher than the maximum internal pressure of the conventional polydimethylsiloxane (PDMS)–glass or PDMS–PDMS bonding. The demonstrated laser process can be applied to produce a new class of glass devices with reliability in a high pressure environment, which cannot be achieved by PDMS devices or ultraviolet (UV) glued glass devices. MDPI 2018-12-03 /pmc/articles/PMC6315772/ /pubmed/30513880 http://dx.doi.org/10.3390/mi9120639 Text en © 2018 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Kim, Sungil
Kim, Jeongtae
Joung, Yeun-Ho
Choi, Jiyeon
Koo, Chiwan
Bonding Strength of a Glass Microfluidic Device Fabricated by Femtosecond Laser Micromachining and Direct Welding
title Bonding Strength of a Glass Microfluidic Device Fabricated by Femtosecond Laser Micromachining and Direct Welding
title_full Bonding Strength of a Glass Microfluidic Device Fabricated by Femtosecond Laser Micromachining and Direct Welding
title_fullStr Bonding Strength of a Glass Microfluidic Device Fabricated by Femtosecond Laser Micromachining and Direct Welding
title_full_unstemmed Bonding Strength of a Glass Microfluidic Device Fabricated by Femtosecond Laser Micromachining and Direct Welding
title_short Bonding Strength of a Glass Microfluidic Device Fabricated by Femtosecond Laser Micromachining and Direct Welding
title_sort bonding strength of a glass microfluidic device fabricated by femtosecond laser micromachining and direct welding
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6315772/
https://www.ncbi.nlm.nih.gov/pubmed/30513880
http://dx.doi.org/10.3390/mi9120639
work_keys_str_mv AT kimsungil bondingstrengthofaglassmicrofluidicdevicefabricatedbyfemtosecondlasermicromachininganddirectwelding
AT kimjeongtae bondingstrengthofaglassmicrofluidicdevicefabricatedbyfemtosecondlasermicromachininganddirectwelding
AT joungyeunho bondingstrengthofaglassmicrofluidicdevicefabricatedbyfemtosecondlasermicromachininganddirectwelding
AT choijiyeon bondingstrengthofaglassmicrofluidicdevicefabricatedbyfemtosecondlasermicromachininganddirectwelding
AT koochiwan bondingstrengthofaglassmicrofluidicdevicefabricatedbyfemtosecondlasermicromachininganddirectwelding