Embrittlement Due to Excess Heat Input into Friction Stir Processed 7075 Alloy
The grain size of high strength 7075 hot-rolled aluminum plates was refined by a friction stir process (FSP) to improve their mechanical properties. The results of the tensile ductility tests, which were conducted at various tool rotational speeds, in the friction stir zone indicate significant tens...