Remaining Life Assessment for Steel After Low-Cycle Fatigue by Surface Crack Image

After pre-fatigue cycles at different strain amplitudes with different N/N(f) values (33.3%, 50%, and 75%), specimens of HRB335 steel were subjected to uniaxial tension until failure. By this method the mechanical properties of the specimens after pre-fatigue testing were measured, and the fracture...