Cargando…

Binder jet additive manufacturing method to fabricate near net shape crack-free highly dense Fe-6.5 wt.% Si soft magnets()

High silicon (Si) electrical steel has the potential for efficient use in applications such as electrical motors and generators with cost-effective in processing, but it is difficult to manufacture. Increasing the Si content beyond 3 wt.% improves magnetic and electrical properties, with 6.5 wt.% be...

Descripción completa

Detalles Bibliográficos
Autores principales: Cramer, Corson L., Nandwana, Peeyush, Yan, Jiaqiang, Evans, Samuel F., Elliott, Amy M., Chinnasamy, Chins, Paranthaman, M. Parans
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Elsevier 2019
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6872844/
https://www.ncbi.nlm.nih.gov/pubmed/31768437
http://dx.doi.org/10.1016/j.heliyon.2019.e02804