Growth, Stratification, and Liberation of Phosphorus-Rich C(2)S in Modified BOF Steel Slag

Basic oxygen furnace (BOF) slag was modified by adding 3.5% SiO(2) and holding at 1673 K for 0, 5, 40, 90, 240, or 360 min. Kilo-scale modification was also carried out. The growth, stratification, and liberation of P-rich C(2)S in the modified slag were investigated. The optimum holding time was 24...