Growth, Stratification, and Liberation of Phosphorus-Rich C(2)S in Modified BOF Steel Slag
Basic oxygen furnace (BOF) slag was modified by adding 3.5% SiO(2) and holding at 1673 K for 0, 5, 40, 90, 240, or 360 min. Kilo-scale modification was also carried out. The growth, stratification, and liberation of P-rich C(2)S in the modified slag were investigated. The optimum holding time was 24...
Autores principales: | Rao, Lei, Dong, Yuanchi, Gui, Mancheng, Zhang, Yaohui, Shen, Xingmei, Wu, Xingrong, Cao, Fabin |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6981783/ https://www.ncbi.nlm.nih.gov/pubmed/31947760 http://dx.doi.org/10.3390/ma13010203 |
Ejemplares similares
-
Using Carbonated BOF Slag Aggregates in Alkali-Activated Concretes
por: Mastali, Mohammad, et al.
Publicado: (2019) -
BOF steel slag as a low-cost sorbent for vanadium (V) removal from soil washing effluent
por: Gao, Yuchen, et al.
Publicado: (2017) -
Geometric Characteristics of BOF Slag Coarse Aggregate and its Influence on Asphalt Concrete
por: Kong, Dezhi, et al.
Publicado: (2019) -
Research Progress on Skid Resistance of Basic Oxygen Furnace (BOF) Slag Asphalt Mixtures
por: Li, Song, et al.
Publicado: (2020) -
Blended Cement Mixed with Basic Oxygen Steelmaking Slag (BOF) as an Alternative Green Building Material
por: Jexembayeva, Assel, et al.
Publicado: (2020)