A Two-Step Annealing Method to Enhance the Pyroelectric Properties of Mn:PIMNT Chips for Infrared Detectors
Mn:0.15Pb(In(1/2)Nb(1/2))O(3)-0.55Pb(Mg(1/3)Nb(2/3))O(3)-0.30PbTiO(3) (Mn:PIMNT) pyroelectric chips were prepared by a two-step annealing method. For the two steps, annealing temperatures dependence of microstructure, defects, surface stress, surface roughness, dielectric properties and pyroelectric...