Co-dosing Ozone and Deionized Water as Oxidant Precursors of ZnO Thin Film Growth by Atomic Layer Deposition

Characteristics of atomic layer deposition (ALD)-grown ZnO thin films on sapphire substrates with and without three-pulsed ozone (O(3)) as oxidant precursor and post-deposition thermal annealing (TA) are investigated. Deposition temperature and thickness of ZnO epilayers are 180 °C and 85 nm, respec...

Descripción completa

Detalles Bibliográficos
Autores principales: Cheng, Yung-Chen, Wang, Hsiang-Chen, Feng, Shih-Wei, Li, Tsai-Pei, Fung, Siu-Keung, Yuan, Kai-Yun, Chen, Miin-Jang
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Springer US 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7391459/
https://www.ncbi.nlm.nih.gov/pubmed/32728964
http://dx.doi.org/10.1186/s11671-020-03382-1
Descripción
Sumario:Characteristics of atomic layer deposition (ALD)-grown ZnO thin films on sapphire substrates with and without three-pulsed ozone (O(3)) as oxidant precursor and post-deposition thermal annealing (TA) are investigated. Deposition temperature and thickness of ZnO epilayers are 180 °C and 85 nm, respectively. Post-deposition thermal annealing is conducted at 300 °C in the ambience of oxygen (O(2)) for 1 h. With strong oxidizing agent O(3) and post-deposition TA in growing ZnO, intrinsic strain and stress are reduced to 0.49% and 2.22 GPa, respectively, with extremely low background electron concentration (9.4 × 10(15) cm(−3)). This is originated from a lower density of thermally activated defects in the analyses of thermal quenching of the integrated intensity of photoluminescence (PL) spectra. TA further facilitates recrystallization forming more defect-free grains and then reduces strain and stress state causing a remarkable decrease of electron concentration and melioration of surface roughness.