Effect of in situ VSi(2) and SiC phases on the sintering behavior and the mechanical properties of HfB(2)-based composites

In situ HfB(2)–SiC–VSi(2) composite was fabricated by reactive pressureless sintering at the temperature of 2150 °C for 4 h under a vacuum atmosphere. In situ SiC and VSi(2) reinforcements were formed using VC and Si powders as starting materials according to the following reaction: VC + 3Si = SiC +...