Cargando…
Effect of in situ VSi(2) and SiC phases on the sintering behavior and the mechanical properties of HfB(2)-based composites
In situ HfB(2)–SiC–VSi(2) composite was fabricated by reactive pressureless sintering at the temperature of 2150 °C for 4 h under a vacuum atmosphere. In situ SiC and VSi(2) reinforcements were formed using VC and Si powders as starting materials according to the following reaction: VC + 3Si = SiC +...
Autores principales: | Ghadami, Soheil, Taheri-Nassaj, Ehsan, Baharvandi, Hamid Reza, Ghadami, Farzin |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Nature Publishing Group UK
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7538434/ https://www.ncbi.nlm.nih.gov/pubmed/33024140 http://dx.doi.org/10.1038/s41598-020-73295-7 |
Ejemplares similares
-
Improvement of mechanical properties of HfB(2)-based composites by incorporating in situ SiC reinforcement through pressureless sintering
por: Ghadami, S., et al.
Publicado: (2021) -
αSiC - βSiC - graphene composites
por: Razmjoo, Ali, et al.
Publicado: (2023) -
Oxidation of Ceramic Materials Based on HfB(2)-SiC under the Influence of Supersonic CO(2) Jets and Additional Laser Heating
por: Simonenko, Elizaveta P., et al.
Publicado: (2023) -
Investigation of the Effect of Supersonic Flow of Dissociated Nitrogen on ZrB(2)–HfB(2)–SiC Ceramics Doped with 10 vol.% Carbon Nanotubes
por: Simonenko, Elizaveta P., et al.
Publicado: (2022) -
Effect of In Situ Grown SiC Nanowires on the Pressureless Sintering of Heterophase Ceramics TaSi(2)-TaC-SiC
por: Vorotilo, Stepan, et al.
Publicado: (2020)