Effect of Post-Weld Annealing on Microstructure and Growth Behavior of Copper/Aluminum Friction Stir Welded Joint

Friction stir welding of 1016 pure aluminum and T2 pure copper with 2 mm thickness was carried out in the form of lap welding of copper on the upper side and aluminum on the lower side. The growth of interface microstructure between 1016 pure aluminum and T2 pure copper welded by friction stir weldi...