Hot Deformation Behavior and Workability of In-Situ TiB(2)/7050Al Composites Fabricated by Powder Metallurgy

Isothermal compression tests of in-situ TiB(2)/7050Al composites fabricated by powder metallurgy were performed at 300–460 °C with the strain rate varying from 0.001 s(−1) to 1 s(−1). The Arrhenius constitutive equation and hot processing map of composites were established, presenting excellent hot...