Dry Sliding Behavior of an Aluminum Alloy after Innovative Hard Anodizing Treatments

This work evaluates the dry sliding behavior of anodic aluminum oxides (AAO) formed during one traditional hard anodizing treatment (HA) and two golden hard anodizing treatments (named G and GP, respectively) on a EN AW-6060 aluminum alloy. Three different thicknesses of AAO layers were selected: 25...

Descripción completa

Detalles Bibliográficos
Autores principales: Soffritti, Chiara, Fortini, Annalisa, Nastruzzi, Anna, Sola, Ramona, Merlin, Mattia, Garagnani, Gian Luca
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8231905/
https://www.ncbi.nlm.nih.gov/pubmed/34198569
http://dx.doi.org/10.3390/ma14123281