Effect of VN and TiB(2)-TiC(x) Reinforcement on Wear Behavior of Al 7075-Based Composites

Al 7075 alloy, 15 wt.% VN/7075 composites, and 20 wt.% TiB(2)-TiC(x)/7075 composites were prepared by ball milling with subsequent hot-pressing sintering. The microstructure, hardness, and wear properties at room temperature to 200 °C of Al 7075-based composites with different reinforcement phases w...