Reaction Sintering of Biocompatible Al(2)O(3)–hBN Ceramics
[Image: see text] Biocompatible Al(2)O(3)–hBN ceramic was sintered from AlN and B(2)O(3) precursors by reaction hot pressing at 1750 °C and 30 MPa for 8 min. The ceramic was compared to nonreactive (NR) one sintered from Al(2)O(3) and BN under the same sintering conditions. The NR ceramic possesses...