Cargando…

Hot Deformation Behavior and Microstructural Evolution Based on the Processing Map of Dual-Phase Mg-Li Based Alloy

The deformation behavior of the as-extruded Mg-Li-Al-Zn-Si alloy was studied by conducting a hot compression test, with a temperature range of 180–330 °C and a strain rate range of 0.01–10 s(−1). The constitutive relationship of flow stress, temperature, and strain rate was expressed by the Zener–Ho...

Descripción completa

Detalles Bibliográficos
Autores principales: Guo, Jiangtao, Guo, Shengli, Shen, Yazhao, Li, Defu
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2022
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8839511/
https://www.ncbi.nlm.nih.gov/pubmed/35160967
http://dx.doi.org/10.3390/ma15031022