Effect of Holding Time on Densification, Microstructure and Selected Properties of Spark Plasma Sintered AA7075-B(4)C Composites

The paper presents the effect of the holding time, varying between 1 min 15 s and 10 min, on the microstructure evolution and development of selected properties of spark plasma sintered AA7075-based composites reinforced with 3, 5 and 10 wt% sub-micro B(4)C powder. The sintering temperature and the...