Reactive intermediate phase cold sintering in strontium titanate

Dense (>96% theoretical) strontium titanate ceramics were fabricated at 950 °C (conventional sintering temperature > 1400 °C) using a reactive intermediate phase cold sintering process. An aqueous solution of SrCl(2) mixed with TiO(2) nanoparticles was added to SrTiO(3) powders and pressed at...