Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions
A lithium-ion battery (LIB) may experience overcharge or over-discharge when it is used in a battery pack because of capacity variation of different batteries in the pack and the difficulty of maintaining identical state of charge (SOC) of every single battery. A series of experiments were establish...