Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions
A lithium-ion battery (LIB) may experience overcharge or over-discharge when it is used in a battery pack because of capacity variation of different batteries in the pack and the difficulty of maintaining identical state of charge (SOC) of every single battery. A series of experiments were establish...
Autores principales: | , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Royal Society of Chemistry
2018
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9086475/ https://www.ncbi.nlm.nih.gov/pubmed/35548129 http://dx.doi.org/10.1039/c8ra05564e |
_version_ | 1784704009543614464 |
---|---|
author | Ouyang, Dongxu Chen, Mingyi Liu, Jiahao Wei, Ruichao Weng, Jingwen Wang, Jian |
author_facet | Ouyang, Dongxu Chen, Mingyi Liu, Jiahao Wei, Ruichao Weng, Jingwen Wang, Jian |
author_sort | Ouyang, Dongxu |
collection | PubMed |
description | A lithium-ion battery (LIB) may experience overcharge or over-discharge when it is used in a battery pack because of capacity variation of different batteries in the pack and the difficulty of maintaining identical state of charge (SOC) of every single battery. A series of experiments were established to investigate the thermal and fire characteristics of a commercial LIB under overcharge/over-discharge failure conditions. According to the results, it is clear that the batteries experienced a clear temperature rise in the overcharge/over-discharge process. The temperature rise worsened and required less time when the battery was overcharged/over-discharged to failure with the increasing charge/discharge rate. Besides, the closer the position to the opening of the battery, the higher the surface temperature. It was demonstrated that LIBs can fail when overcharged/over-discharged to a critical degree regardless of the charge/discharge rate. Under different rates, the final capacities were around a critical value. Finally, there existed an explosion phenomenon in the external heating test of battery failure after overcharge, whereas the fire behaviors of the over-discharged battery were much more moderate. |
format | Online Article Text |
id | pubmed-9086475 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2018 |
publisher | The Royal Society of Chemistry |
record_format | MEDLINE/PubMed |
spelling | pubmed-90864752022-05-10 Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions Ouyang, Dongxu Chen, Mingyi Liu, Jiahao Wei, Ruichao Weng, Jingwen Wang, Jian RSC Adv Chemistry A lithium-ion battery (LIB) may experience overcharge or over-discharge when it is used in a battery pack because of capacity variation of different batteries in the pack and the difficulty of maintaining identical state of charge (SOC) of every single battery. A series of experiments were established to investigate the thermal and fire characteristics of a commercial LIB under overcharge/over-discharge failure conditions. According to the results, it is clear that the batteries experienced a clear temperature rise in the overcharge/over-discharge process. The temperature rise worsened and required less time when the battery was overcharged/over-discharged to failure with the increasing charge/discharge rate. Besides, the closer the position to the opening of the battery, the higher the surface temperature. It was demonstrated that LIBs can fail when overcharged/over-discharged to a critical degree regardless of the charge/discharge rate. Under different rates, the final capacities were around a critical value. Finally, there existed an explosion phenomenon in the external heating test of battery failure after overcharge, whereas the fire behaviors of the over-discharged battery were much more moderate. The Royal Society of Chemistry 2018-09-27 /pmc/articles/PMC9086475/ /pubmed/35548129 http://dx.doi.org/10.1039/c8ra05564e Text en This journal is © The Royal Society of Chemistry https://creativecommons.org/licenses/by-nc/3.0/ |
spellingShingle | Chemistry Ouyang, Dongxu Chen, Mingyi Liu, Jiahao Wei, Ruichao Weng, Jingwen Wang, Jian Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions |
title | Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions |
title_full | Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions |
title_fullStr | Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions |
title_full_unstemmed | Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions |
title_short | Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions |
title_sort | investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions |
topic | Chemistry |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC9086475/ https://www.ncbi.nlm.nih.gov/pubmed/35548129 http://dx.doi.org/10.1039/c8ra05564e |
work_keys_str_mv | AT ouyangdongxu investigationofacommerciallithiumionbatteryunderoverchargeoverdischargefailureconditions AT chenmingyi investigationofacommerciallithiumionbatteryunderoverchargeoverdischargefailureconditions AT liujiahao investigationofacommerciallithiumionbatteryunderoverchargeoverdischargefailureconditions AT weiruichao investigationofacommerciallithiumionbatteryunderoverchargeoverdischargefailureconditions AT wengjingwen investigationofacommerciallithiumionbatteryunderoverchargeoverdischargefailureconditions AT wangjian investigationofacommerciallithiumionbatteryunderoverchargeoverdischargefailureconditions |